Techno-Economic Issues in Materials Selection

By
Joel P. Clark
Joel P. Clark
Massachusetts Institute of Technology
Search for other works by this author on:
;
Richard Roth
Richard Roth
Massachusetts Institute of Technology
Search for other works by this author on:
;
Frank R. Field, III
Frank R. Field, III
Massachusetts Institute of Technology
Search for other works by this author on:
Published:
1997
Page range:
255 - 265

Abstract

This article provides an overview of cost analysis in materials selection. It discusses the several categories of alternatives for cost analysis. These include rules of thumb, accounting methods, and analytical methods. The article describes the methods for evaluating materials alternatives on the basis of costs, both direct economic costs and indirect social costs. It discusses the life cycle costs of alternative body-in-white designs and life cycle analysis.The various elements of cost are introduced with a case study concerned with the manufacture, use, and disposal of the automobile body-in-white.

You do not currently have access to this content.
Don't already have an account? Register

Joel P. Clark, Richard Roth, Frank R. Field, III, 1997. "Techno-Economic Issues in Materials Selection", Materials Selection and Design, George E. Dieter

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal