Materials Selection and Design
Metal Additive Manufacturing—A Review[1][2]
-
Published:1997
Abstract
This article reviews the emerging manufacturing technology that is alternatively called additive manufacturing (AM), direct digital manufacturing, free-form fabrication, three-dimensional (3-D) printing, and so on. It provides a broad contextual overview of metallic AM. The article focuses on the mechanical properties of AM-processed Ti-6Al-4V, IN-625, and IN-718. The development of closed-loop, real-time, sensing, and control systems is essential to the qualification and advancement of AM. This involves the development of coupled process-microstructural models, sensor technology, and control methods and algorithms. AM has the potential to revolutionize the global parts manufacturing and logistics landscape. It enables distributed manufacturing and the productions of parts on demand while offering the potential to reduce cost, energy consumption, and carbon footprint. The article explores the materials science, processes, and business considerations associated with achieving these performance gains. It concludes that a paradigm shift is required to fully exploit AM potential.
Sign in
ASM members
Member Sign InWilliam E. Frazier, Metal Additive Manufacturing—A Review, Materials Selection and Design, Vol 20, ASM Handbook, Edited By George E. Dieter, ASM International, 1997, p 1–9, https://doi.org/10.31399/asm.hb.v20.a0009211
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.