This article focuses on the modeling and simulation of diffusion-controlled processes related to both materials processing such as heat treatments, and materials degradation from a practical perspective by using the one-dimensional (1-D) sharp interface approach. It describes various diffusion simulation models, such as one-phase simulations, moving phase-boundary simulations, and dispersed system simulations. The article presents case studies that illustrate some examples where diffusion simulations have been applied to industrial-based problems, with an emphasis on the approaches used and the lessons learned from performing such simulations.