Metals Process Simulation
Software for Computational Materials Modeling and Simulation
-
Published:2010
Abstract
This article demonstrates the depth and breadth of commercial and third-party software packages available to simulate metals processes. It provides a representation of the spectrum of applications from simulation of atomic-level effects to manufacturing optimization. The article tabulates the software name, function or process applications, vendor or developer, and website information.
Sign in
ASM members
Member Sign InSoftware for Computational Materials Modeling and Simulation, Metals Process Simulation, Vol 22B, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2010, p 649–656, https://doi.org/10.31399/asm.hb.v22b.a0005544