Abstract

The most popular metal hot working processes for which induction heating is applied are forging, forming, extrusion, and rolling. This article focuses on estimation techniques to determine basic induction heating process parameters, including coil power, length of heating line, and frequency selection. It discusses three modes of heat transfer: conduction, convection, and radiation, in induction heating. The article describes the factors affected by a distortion of the magnetic field at the coil end through a schematic illustration of distribution of three magnetic force components experienced by the turns of the coil. It concludes with information on some case studies of numerical simulation.

You do not currently have access to this chapter.
Don't already have an account? Register

Simulation of Heat Treatment Processes, Metals Process Simulation, Vol 22B, ASM Handbook, Edited By D.U. Furrer, S.L. Semiatin, ASM International, 2010

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal