This article reviews network models and their applications for the simulation of various physical phenomena related to grain-boundary migration. It discusses the steps involved in the implementation of two and three-dimensional network models, namely, acquisition and discretization of the microstructure, formulation of the equation of motion, and implementation of the topological transformations. The article presents examples that illustrate the simulation of physical phenomena to demonstrate the predictive power and flexibility of network models.