This article is a comprehensive collection of fluid dynamic equations for properties of fluids, fluid statics, fluid motion, dimensional analysis, and boundary layer flow. It presents equations for analyzing problems in fluid mechanics, continuity equation, momentum equation, and energy equation for solving various problems related to fluid dynamics.