Integrated Computational Materials Engineering[1]

By
John E. Allison
John E. Allison
Ford Motor Company
Search for other works by this author on:
;
Mei Li
Mei Li
Ford Motor Company
Search for other works by this author on:
;
XuMing Su
XuMing Su
Ford Motor Company
Search for other works by this author on:
Published:
2009
Page range:
7 - 14
Publication history
July 13, 2009

Abstract

Integrated computational materials engineering refers to the use of computer simulations that integrate mathematical models of complex metallurgical processes with computer models used in component and process design. This article outlines an example of a computer-aided engineering tool, such as virtual aluminum castings (VAC), developed and implemented for quickly developing durable cast aluminum power train components. It describes the procedures for the model development of the VAC system. These procedures include linking the manufacturing process to microstructure, linking microstructures to mechanical properties, linking material properties to performance prediction, and model validation and integration into the engineering process. The article discusses the benefits of the VAC system in process selection, process optimization, and improving the component design criteria.

You do not currently have access to this content.
Don't already have an account? Register

John E. Allison, Mei Li, XuMing Su, 2009. "Integrated Computational Materials Engineering", Fundamentals of Modeling for Metals Processing, D.U. Furrer, S.L. Semiatin

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal