Abstract

This article is a comprehensive collection of the thermodynamic equations and property relations of the first and second laws of thermodynamics that are applicable to closed-system consisting of several homogeneous and heterogeneous phases.

You do not currently have access to this chapter.
Don't already have an account? Register

2009. "Thermodynamics", Fundamentals of Modeling for Metals Processing, D.U. Furrer, S.L. Semiatin