Abstract

This article presents the Schmid's law that describes the response of crystal structures to loading. It describes the Taylor model to calculate the uniaxial yield stress of an isotropic face-centered cubic aggregate in terms of critical resolved shear stress. The article discusses the stress-based approach of the Bishop and Hill procedure to directly find stress states that could simultaneously operate at least five independent slip systems. It presents ways to find isostress or lower-bound yield loci for sheets having single-crystal orientation.

You do not currently have access to this chapter.
Don't already have an account? Register

Henry R. Piehler, 2009. "Crystal-Plasticity Fundamentals", Fundamentals of Modeling for Metals Processing, D.U. Furrer, S.L. Semiatin