This article focuses on the analysis of materials and mechanical- (or biomechanical-) based medical device failures. It reviews the failure analysis practices, including evidence receipt, cleaning, nondestructive examination, destructive examination, exemplars analysis, and device redesign. The article examines the common failure modes, such as overload, fatigue, corrosion, hydrogen embrittlement, and fretting, of medical devices. The failure analysis of orthopedic implants, such as permanent prostheses and internal fixation devices, is described. The article reviews the failure mechanisms in some of the more common medical device materials, namely, stainless steels, titanium alloys, cobalt-base alloys, and nitinol. It presents case histories with examples for failure analysis.

You do not currently have access to this chapter.
Don't already have an account? Register

Brad A. James, 2012. "Medical Device Failure Analysis", Materials for Medical Devices, Roger J. Narayan

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal