Abstract

This article reviews the friction and wear of various dental materials that have been studied by fundamental wear measurements, simulated service wear measurements, and clinical measurements. The materials include dental amalgam, composite restorative materials, pit and fissure sealants, dental cements, porcelain and plastic denture teeth, dental feldspathic porcelain and ceramics, endodontic instruments, periodontal Instruments, and orthodontic wires. The article describes the correlations of properties, such as hardness, fracture toughness, and wear. It discusses wear mechanism such as sliding adhesive wear, two-body abrasion, three-body abrasion, erosion, and fatigue.