This article reviews the corrosion interactions between biomedical alloys, in particular iron-base, titanium-base, and cobalt-base alloys, in complex geometries and in applications where there are significant cyclic stresses and potential for wear and fretting motion. It discusses the nature of these metal surfaces and their propensity for corrosion reactions when combined with similar or different alloys in complex restrictive environments within the human body, and under loading conditions. The article describes factors that influence mechanically assisted crevice corrosion. It reviews tests, such as scratch test and in vitro fretting corrosion test, developed to investigate the aspects of mechanically assisted corrosion of metallic biomaterials.

You do not currently have access to this chapter.
Don't already have an account? Register

2012. "Mechanically Assisted Corrosion of Metallic Biomaterials", Materials for Medical Devices, Roger J. Narayan

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal