This article discusses the composition of major components of dental composite resins. The components include organic resin matrix, filler, coupling agents, and initiator-accelerator systems. The article provides a description of three steps in adhesive systems, namely, etching, priming, and the placement of a resin adhesive layer. It describes the properties of composite resins that are related to the amount and type of filler and resin-matrix compositions. The article also provides a discussion on the compositions, properties, and clinical applications of polyacid-modified composite resins and resin-modified glass-ionomer cements. It discusses the biodegradation and biocompatibility of resin-based restorative materials.

You do not currently have access to this chapter.
Don't already have an account? Register

Yoav Finer, 2012. "Dental Composite Resins", Materials for Medical Devices, Roger J. Narayan

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal