This article provides a summary of biocompatibility or biological response of metals, ceramics, and polymers used in medical implant, along with their clinical issues. The polymers include ultrahigh-molecular-weight polyethylene, nonresorbable polymer, and resorbable polymers.

Abstract

The biocompatibility of a material relates to its immunological response, toxicity profile, and ability to integrate with surrounding tissue without undesirable local or systemic effects on a patient. This article underscores the transformation of the medical device design ecosystem engaged as an integral part of the device ecosystem. It discusses the various applications of biomaterials, including orthopedic, cardiovascular, ophthalmic, and dental applications. The article describes the four major categories of biomaterials, such as metals, polymers, glass and ceramics, and composites. A discussion on natural materials, nanomaterials, and stem cells is also provided. The article concludes with information on examples of biomaterials applications, including endovascular devices, knee implants, and neurostimulation.

You do not currently have access to this chapter.
Don't already have an account? Register

2012. "Introduction", Materials for Medical Devices, Roger J. Narayan

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal