Abstract
The biocompatibility of a material relates to its immunological response, toxicity profile, and ability to integrate with surrounding tissue without undesirable local or systemic effects on a patient. This article underscores the transformation of the medical device design ecosystem engaged as an integral part of the device ecosystem. It discusses the various applications of biomaterials, including orthopedic, cardiovascular, ophthalmic, and dental applications. The article describes the four major categories of biomaterials, such as metals, polymers, glass and ceramics, and composites. A discussion on natural materials, nanomaterials, and stem cells is also provided. The article concludes with information on examples of biomaterials applications, including endovascular devices, knee implants, and neurostimulation.
Sign in
ASM members
Member Sign InColin K. Drummond, Alia Hdeib, Fahd R. Khan, Applications of Medical Implant Materials, Materials for Medical Devices, Vol 23, ASM Handbook, Edited By Roger J. Narayan, ASM International, 2012, p 18–35, https://doi.org/10.31399/asm.hb.v23.a0005660
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.