A number of nondestructive evaluation (NDE) methods, such as radiography, ultrasound, and eddy current, are available to detect flaws in solid materials. This article describes the fundamental aspects of these NDE methods in terms of operation principles. It presents some examples of the methods performed on various types of flaws resulting from solid-state welding processes.