Castability of alloys is a measure of their ability to be cast to a given shape with a given process without the formation of cracks/tears, pores/shrinkage, and/or other significant casting defects. This article discusses the factors which affect the fluidity of an iron melt: alloy composition and initial melt condition. Besides the basic alloy properties, the effective castability of high-alloy irons can be significantly improved through casting and casting system design. The article describes the product design and processing factors of high-alloy graphitic irons and high-alloy white irons. It explains the heat treatment of high-silicon irons for high-temperature service and concludes with a discussion on machining and finishing of high-alloy iron castings.

You do not currently have access to this chapter.
Don't already have an account? Register

Harry Tian, Richard B. Gundlach, 2017. "Castability, Product Design, and Production of High-Alloy Iron Castings", Cast Iron Science and Technology, Doru M. Stefanescu

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal