The Austenite-to-Pearlite/Ferrite Transformation

By
Jacques Lacaze
Jacques Lacaze
Université de Toulouse
Search for other works by this author on:
Published:
2017
Page range:
106 - 113
Publication history
August 28, 2017

Abstract

This article discusses the stable and metastable three-phase fields in the binary Fe-C phase diagram. It schematically illustrates that austenite decomposition requires accounting for nucleation and growth of ferrite and then nucleation and growth of pearlite in the remaining untransformed volume. The article describes the austenite decomposition to ferrite and pearlite in spheroidal graphite irons and lamellar graphite irons. It provides a discussion on modeling austenite decomposition to ferrite and pearlite.

You do not currently have access to this content.
Don't already have an account? Register

Jacques Lacaze, 2017. "The Austenite-to-Pearlite/Ferrite Transformation", Cast Iron Science and Technology, Doru M. Stefanescu

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal