Abstract

This article discusses the characterization of gray iron structures, following the sequence of structure formation, as it applies to unalloyed or low-alloyed gray iron. Austenite grains are the basic crystallographic entities of the metallic matrix in gray cast iron precipitated from the liquid melt. The article describes the macrostructure and dendrite morphology of primary austenite. Eutectoid transformation in the solid state causes the transformation of austenite to pearlite and/or ferrite, producing the as-cast structure. The article discusses the observations of the graphite and ferritic/pearlitic structure in as-cast gray iron.

You do not currently have access to this chapter.
Don't already have an account? Register

Attila Diószegi, Lucian Vasile Diaconu, Microstructures and Characterization of Gray Irons, Cast Iron Science and Technology, Vol 1A, ASM Handbook, Edited By Doru M. Stefanescu, ASM International, 2017, p 583–589, https://doi.org/10.31399/asm.hb.v01a.a0006343

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal