Abstract

As cast iron parts are extensively applied, fracture events will eventually take place. Consequently, it becomes essential to carry out failure analyses to identify the cause of fracture and to provide corrective actions that allow safe operation. This article presents a description of the main fracture modes and their characteristic fractographic features. It discusses the four principal fracture modes: dimple rupture (or fracture), cleavage, fatigue, and intergranular fracture. The article provides information on special cases of environmentally assisted fracture. It concludes with a description of fractographic analyses for identifying the direction of propagation of a crack.

You do not currently have access to this chapter.
Don't already have an account? Register

Diego O. Fernandino, Roberto E. Boeri, Fracture Analysis, Cast Iron Science and Technology, Vol 1A, ASM Handbook, Edited By Doru M. Stefanescu, ASM International, 2017, p 399–410, https://doi.org/10.31399/asm.hb.v01a.a0006323

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal