Cast irons, like steels, are iron-carbon alloys but with higher carbon levels than steels to take advantage of eutectic solidification in the binary iron-carbon system. This article introduces the solid-state heat treatment of iron castings and describes the various processes of heat treatment of cast iron. It provides information on stress relieving, annealing, normalizing, through hardening, and surface hardening of these castings. The article discusses general considerations for the heat treatment of cast iron. Cast irons are occasionally nitrided for various applications with the aim of enhancing surface hardness and corrosion resistance of the products. The article describes molten salt bath cyaniding and ion nitriding of cast iron.

You do not currently have access to this chapter.
Don't already have an account? Register

J.L. Dossett, Introduction to Cast Iron Heat Treatment, Cast Iron Science and Technology, Vol 1A, ASM Handbook, Edited By Doru M. Stefanescu, ASM International, 2017, p 228–239, https://doi.org/10.31399/asm.hb.v01a.a0006296

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal