Abstract

Thin-wall gray cast iron (TWGCI) can be seen as a potential material for the preparation of lightweight castings in automotive engineering applications. This article discusses the most important challenges for TWGCI: cooling rate, solidification, macrostructure, microstructure, and chilling tendency. It reviews the tensile properties and thermophysical properties of gray cast iron. The article describes the variables that influence molten iron preparation: charge materials, melting furnace thermal regime, chemical composition, modification and inoculation treatment, holding time/pouring procedure, mold properties (mold temperature, thermophysical properties of mold and mold coating), and casting design.

You do not currently have access to this chapter.
Don't already have an account? Register

Marcin Górny, Thin-Wall Gray Iron Castings, Cast Iron Science and Technology, Vol 1A, ASM Handbook, Edited By Doru M. Stefanescu, ASM International, 2017, p 575–582, https://doi.org/10.31399/asm.hb.v01a.a0006316

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal