Compacted graphite iron (CGI) invariably includes some nodular (spheroidal) graphite particles, giving rise to the definition of the microstructure in terms of percent nodularity. This article discusses the graphite morphology and mechanical and physical properties of CGI. The mechanical and physical properties of CGI with ferritic and pearlitic matrix structures are summarized in a table. The article describes the standards for CGI, with the definition of the grades based on the minimum tensile strength. It also provides information on the applications of compacted graphite iron castings.

You do not currently have access to this chapter.
Don't already have an account? Register

Steve Dawson, Wilson Guesser, Specification, Selection, and Applications of Compacted Graphite Irons, Cast Iron Science and Technology, Vol 1A, ASM Handbook, Edited By Doru M. Stefanescu, ASM International, 2017, p 659–664, https://doi.org/10.31399/asm.hb.v01a.a0006312

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal