Skip to Main Content
Skip Nav Destination

Abstract

Solidification of cast iron alloys brings about volumetric changes. This article describes direct measurements of volume changes with an illustration of the analysis of volumetric changes during solidification of cast iron with the use of a specially designed riser combined with a furnace. It provides a discussion on the dilatometer analysis that is generally used to measure linear displacement as a function of temperature for all types of materials, and the problems associated with volume-change measurements. The article presents a graphical representation of a consequence of the anisotropy, where the calculated volume change is illustrated as a function of temperature. It concludes with a review of kinetic of graphite expansion.

You do not currently have access to this chapter.
Don't already have an account? Register

Attila Diószegi, Volumetric Changes during the Solidification of Cast Iron, Cast Iron Science and Technology, Vol 1A, ASM Handbook, Edited By Doru M. Stefanescu, ASM International, 2017, p 88–93, https://doi.org/10.31399/asm.hb.v01a.a0006330

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal