Abstract

The microstructure that develops during the solidification stage of cast iron largely influences the subsequent solid-state transformations and mechanical properties of the cast components. This article provides a brief introduction of methods that can be used for simulating the solidification microstructure of cast iron. Analytical as well as numerical models describing solidification phenomena at both macroscopic and microscopic scales are presented. The article introduces macroscopic transport equations and presents analytical microscopic models for solidification. These models include the dendrite growth models and the cooperative eutectic growth models. The article provides some solutions using numerical models to simulate the kinetics of microstructure formation in cast iron. It concludes with a discussion on cellular automaton (CA) technique that can handle complex topology changes and reproduce most of the solidification microstructure features observed experimentally.

You do not currently have access to this chapter.
Don't already have an account? Register

A.V. Catalina, A.A. Burbelko, W. Kapturkiewicz, M. Zhu, Computational Models for Prediction of Solidification Microstructure, Cast Iron Science and Technology, Vol 1A, ASM Handbook, Edited By Doru M. Stefanescu, ASM International, 2017, p 94–105, https://doi.org/10.31399/asm.hb.v01a.a0006314

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal