Abstract

This article illustrates typical wear and friction issues encountered in gas and steam turbines and their consequences as well as commonly adopted materials solutions. It contains tables that present the summary of wear and friction related issues encountered in steam turbines and gas turbines. The article outlines the differences in the operating conditions and the nature of the components involved in gas and steam turbines. It discusses the constraints and applicable coating solutions for wear and friction issues, and concludes with a broad set of challenges that need to be addressed to improve performance and operability of gas and steam turbines.

You do not currently have access to this chapter.
Don't already have an account? Register

K. Anand, 2017. "Wear of Steam Turbine and Gas Turbine Components", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal