Tribology is the science and technology of interacting surfaces in relative motion. This article describes in detail the basic structural, operational, and interaction parameters of a tribosystem. The interaction parameters, which characterize the action of the operational parameters on the structural components in the system, consist of three important aspects: contact parameters, friction parameters, and wear parameters. These three aspects embody the complex mechanisms and relationships between the constituents of a tribosystem. The article concludes with information on the selection criteria of a material for wear applications.

You do not currently have access to this chapter.
Don't already have an account? Register

Horst Czichos, Mathias Woydt, 2017. "Introduction to Tribology and Tribological Parameters", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal