Transition metal dichalcogenides (TMD) are solid lubricant materials, specifically, intrinsic solid lubricants, whose crystal structure facilitates interfacial sliding/shear to achieve low friction and wear in sliding contacts and low torque in rolling contacts. This article provides information on sliding friction and wear behavior of unbonded, bonded, and vapor-deposited pure and composite MoS2 and WS2 coatings. It discusses the rolling-torque behavior and applications of vapor-deposited pure and composite MoS2 and WS2 coatings. The article concludes with information on various forms of TMD lubrication, namely, oils, greases, microparticle and nanoparticle additives.

You do not currently have access to this chapter.
Don't already have an account? Register

T.W. Scharf, 2017. "Transition Metal Dichalcogenide-Based (MoS2, WS2) Coatings", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal