Abstract

Strategies for the lubrication of mechanical systems operating in extreme environments must exclude the liquid lubricants and greases and rely on alternative methods of lubrication, such as gases and solids. This article provides a survey of some of the more effective alternative methods of lubrication. It provides a discussion on the solid materials that have been most commonly used as lubricants: carbon-base materials, transition metal dichalcogenides, polymers, and soft metals.

You do not currently have access to this chapter.
Don't already have an account? Register

Gary Doll, 2017. "Lubrication Strategies for Extreme Environments", Friction, Lubrication, and Wear Technology, George E. Totten