This article describes the numerous techniques used to measure friction. It provides a brief description of the historical development of friction testing. The article discusses the tests and equipment available for friction testing. It explains the procedural considerations that should be addressed to ensure that valid data are derived from a friction test. The article presents definitions of terms commonly used in tribology such as static friction, kinetic coefficient of friction, stick-slip behavior, and lubricated friction. It provides information on the precautions that must be taken to ensure valid test results. The article also describes how to report data and how to analyze these data.

You do not currently have access to this chapter.
Don't already have an account? Register

K.G. Budinski, 2017. "Laboratory Testing Methods for Solid Friction", Friction, Lubrication, and Wear Technology, George E. Totten

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal