This article discusses the physical signs of rolling-contact wear (RCW). It lists the major considerations in gear design and describes the mechanisms of RCW. The article provides a guide to rolling-contact fatigue (RCF) testing methods. It explains the steps involved in the processes of RCF and RCW.