Drawing is a process by which a workpiece is pulled against a die to produce a wire, bar, or tube with smaller cross sectional area compared with the initial stock. This article discusses the variables that affect the drawing process and the parameters that influence friction, lubrication, and wear. These parameters include process, lubricant, workpiece, and tooling. The article provides information on dry and wet lubrication in wire drawing. The dry lubrication refers to use of solid lubricants while wet lubrication refers to the practice of providing a liquid lubricant to the workpiece-die interface. The article describes the most...