Friction, Lubrication, and Wear Technology
Frictional Heating in Dry and Lubricated Contacts
-
Published:2017
Abstract
This article provides an overview of experimental, analytical, and numerical tools for temperature evaluation of dry and lubricated systems. It describes the analytical methods and numerical techniques for frictional heating and temperature estimation, as well as viscous heating in full-film lubrication. The article also discusses the viscous heating temperature measurements and numerical analysis of viscous heating.
Sign in
ASM members
Member Sign InJacob Sukumaran, Patrick De Baets, Dieter Fauconnier, Frictional Heating in Dry and Lubricated Contacts, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 67–80, https://doi.org/10.31399/asm.hb.v18.a0006409
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.