This article discusses the classification of wear based on the presence or absence of effective lubricants, namely, lubricated and nonlubricated wear. Variations in ambient temperature, atmosphere, load, and sliding speed, as well as variations in material bulk composition, microstructure, surface treatment, and surface finish of steel are also considered. The article discusses the types, wear testing, wear evaluation, and hardness evaluation of abrasive wear. It describes the selection criteria of steels for wear resistance. The article also describes the importance of hardness and microstructure as factors in resistance to wear. It provides a discussion on the resistance of various...