This article focuses on the tribological behavior of group 1, 2, and 3 cobalt-base alloys, namely, carbide-type wear-resistant alloys and laves-type wear-resistant alloys. The behavior includes hardness, yield strength and ductility, and fracture toughness. The article contains a table that lists the nominal compositions and typical applications of cobalt-base alloys. It discusses the properties and relative performance of specific alloys when subjected to the more common types of wear. These include abrasive wear, high-temperature sliding wear, rolling-contact fatigue wear, and erosive wear.

You do not currently have access to this chapter.
Don't already have an account? Register

Rehan Ahmed, Heidi de Villiers-Lovelock, Friction and Wear of Cobalt-Base Alloys, Friction, Lubrication, and Wear Technology, Vol 18, ASM Handbook, Edited By George E. Totten, ASM International, 2017, p 487–501, https://doi.org/10.31399/asm.hb.v18.a0006390

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal