Abstract

This article provides a detailed account on forming operations (blanking, piercing, press-brake forming, contour rolling, deep drawing, cold forming, and hot forming) of various nonferrous metals, including aluminum alloys, beryllium, copper and its alloys, magnesium alloys, nickel alloys, titanium alloys, and platinum metals. It discusses the formability, equipment and tooling, and lubricants used in the forming operations of these nonferrous metals.

You do not currently have access to this chapter.
Don't already have an account? Register

1998. "Forming of Nonferrous Metals", Metals Handbook Desk Edition, Joseph R. Davis