This article discusses the classifications, specifications, applications and methods for producing welded and seamless steel tubular products, including pipes and tubes. Common types of pipes include standard pipe, conduit pipe, piling pipe, pipe for nipples, transmission or line pipe, water main pipe, oil country tubular goods, water well pipe, and pressure pipe. Pipes in suitable sizes, and most products classified as tubing, both seamless and welded, may be cold finished. Pressure tubes are given a separate classification by both the American Society for Testing and Materials (ASTM) and producers. The term tube covers three groups, including pressure tubes, structural tubing, and mechanical tubing.

You do not currently have access to this chapter.
Don't already have an account? Register

1998. "Steel Tubular Products", Metals Handbook Desk Edition, Joseph R. Davis

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal