Closed-Die Steel Forgings

Published:
1998
Page range:
244 - 248

Abstract

Forging is the process of working hot metal between dies, usually under successive blows and sometimes by continuous squeezing. This article describes the material selection criteria, quality assurance tests for forged components, and the dimensional tolerances of closed-die steel forgings. It provides an overview of the mechanical properties of wrought materials. The article also includes information on the fundamentals of hammer and press forgings and the design of hot upset forgings.

You do not currently have access to this content.
Don't already have an account? Register

1998. "Closed-Die Steel Forgings", Metals Handbook Desk Edition, Joseph R. Davis

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal