This article is a comprehensive collection of machining data, presented in tables, covering most of the commonly used machining operations including turning, face milling, end milling (peripheral), drilling, reaming, and tapping of several materials. It provides starting recommendations for the range of speeds and feeds for various machining operations, parameters for the selection of tool geometry, and guidelines on the selection and identification of cutting fluids.