Abstract

Material properties are the link between the basic structure and composition of the material and the service performance of a part or component. This article describes the most significant properties that must be considered when choosing a metal for a given application, namely physical properties (mass characteristics and thermal, electrical, magnetic, radiation, and optical properties), chemical properties (corrosion and oxidation resistance) and mechanical properties (tensile and yield strength, elongation, toughness, hardness, creep, and fatigue). The article also contains tables that list room-temperature physical properties, vapor pressures, and mechanical properties for various metals.

You do not currently have access to this chapter.
Don't already have an account? Register

Hugh Baker, 1998. "Properties of Metals", Metals Handbook Desk Edition, Joseph R. Davis

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal