Abstract

Arc welding methods can be classified into shielded metal arc welding, flux-cored arc welding, submerged arc welding, gas metal arc welding, gas tungsten arc welding, plasma arc welding, plasma-metal inert gas (MIG) welding, and electroslag and electrogas welding. This article provides information on process capabilities, principles of operation, power sources, electrodes, shielding gases, flux, process variables, and advantages and disadvantages of these arc welding methods. It presents information about the arc welding procedures of hardenable carbon and alloy steels, cast irons, stainless steels, heat-resistant alloys, aluminum alloys, copper and copper alloys, magnesium alloys, nickel alloys, and titanium and titanium alloys.

You do not currently have access to this chapter.
Don't already have an account? Register

1998. "Arc Welding", Metals Handbook Desk Edition, Joseph R. Davis

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal