Abstract

Acoustic-emission inspection detects and analyzes minute acoustic-emission signals generated by discontinuities in materials under applied stress. This article discusses the types of acoustic emissions (continuous-type emissions and burst-type emissions) and applications, including laboratory testing, production testing, and structural testing. The article includes a section in which the characteristics of acoustic emission inspection are compared with other nondestructive testing methods. Further, it briefly reviews the key elements of the acoustic-emission instrumentation, which includes the acoustic-emission resonant sensor.