Rolling-element bearings, whether ball bearings or roller bearings with spherical, straight, or tapered rollers, are fabricated from a wide variety of steels. This article discusses the production process, characteristics, nominal compositions, and types of bearing steels. These include standard bearing steels, such as high-carbon bearing steels and carburizing bearing steels; and special-purpose bearing steels, such as high-temperature service bearing steels and corrosion-resistant bearing steels.