This article discusses the applications and tensile properties of selected copper tube alloys, as well as the methods for producing copper tubular products, namely extrusion and rotary piercing. It explains the methods available for the finishing of copper tubular products, such as tube welding, cold drawing, and tube reducing. The article lists the standard dimensions and tolerances for several kinds of copper tubes and pipes in the ASTM specifications, along with other requirements for the tubular products.