Aluminum alloys are primarily used for nonferrous castings because of their light weight and corrosion resistance. This article discusses at length the melting and metal treatment, structure control, sand casting, permanent mold casting, and die casting of aluminum alloys. It also covers the types and melting and casting practices of copper alloys, zinc alloys, magnesium alloys, titanium alloys, and superalloys, and provides a brief account on the casting technique of metal-matrix composites.
Sign in
ASM members
Member Sign InThomas S. Piwonka, Foundry Practice for Nonferrous Alloys, Metals Handbook Desk Edition, 2nd Ed., 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 771–778, https://doi.org/10.31399/asm.hb.mhde2.a0003175
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.