Solid-State Welding Processes
-
Published:1998
Abstract
This article describes the mechanism, advantages and disadvantages, fundamentals, capabilities, variations, equipment used, and weldability of metals in solid-state welding processes, including diffusion bonding, explosion welding, friction welding, ultrasonic welding, upset welding, and deformation welding.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Solid-State Welding Processes, Metals Handbook Desk Edition, 2nd Ed., 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 1104–1106, https://doi.org/10.31399/asm.hb.mhde2.a0003209
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Book Content
Safe Welding Practices
Welding Fundamentals and Processes
Solid-State Welding and Bonding
Joining Understanding the Basics
Joining of Oxide-Dispersion-Strengthened Materials
Welding, Brazing and Soldering
Safe Practices
Welding, Brazing and Soldering
Welding of Plastics
Welding, Brazing and Soldering
Flash Welding and Upset Welding
Welding Fundamentals and Processes
Upset Welding
Welding, Brazing and Soldering
Procedure Development and Practice Considerations for Resistance Welding
Welding, Brazing and Soldering
Resistance Welding of Aluminum Alloys
Aluminum Science and Technology
Resistance Welding
Joining Understanding the Basics