Abstract

Cobalt finds its use in various applications owing to its magnetic properties, corrosion resistance, wear resistance, and its strength at elevated temperatures. This article discusses the mining and processing of cobalt and cobalt alloys. It describes the types of cobalt alloys, including wear-resistant alloys, high-temperature alloys, corrosion-resistant alloys, and special-purpose alloys. The article provides data on the chemical composition, mechanical properties, and physical properties of these alloys. Further, it provides information on the uses of cobalt in superalloys, cemented carbides, magnetic materials, low-expansion alloys, and high-speed tool steels.