Nickel and nickel-base alloys are vitally important to modern industry because of their ability to withstand a wide variety of severe operating conditions involving corrosive environments, high temperatures, high stresses, and combinations of these factors. This article discusses the mining and extraction of nickel and describes the uses of nickel. It discusses the categories of nickel-base alloys, including wrought corrosion-resistant alloys, cast corrosion-resistant alloys, heat-resistant alloys (superalloys), and special-purpose alloys. The article covers the corrosion resistance of nickel with the inclusion of varying alloying elements. It provides useful information on the behavior of nickel and nickel alloys in specific environments describes its corrosion resistance in certain acids, alkalis, and salts.

You do not currently have access to this chapter.
Don't already have an account? Register

Nickel and Nickel Alloys, Metals Handbook Desk Edition, 2nd Ed., 2nd ed., Edited By Joseph R. Davis, ASM International, 1998, p 609–615, https://doi.org/10.31399/asm.hb.mhde2.a0003147

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal