Abstract

Copper and copper alloys are widely used in many environments and applications because of their excellent corrosion resistance, which is coupled with combinations of other desirable properties. This article lists the identifying characteristics of the forms of corrosion that commonly attack copper metals as well as the most effective means of combating each. General corrosion, galvanic corrosion, pitting, impingement, fretting, intergranular corrosion, dealloying, corrosion fatigue, and stress-corrosion cracking (SCC) are some forms of corrosion. The article also lists a galvanic series of metals and alloys valid for dilute aqueous solutions, such as seawater and weak acids. It provides useful information on the effects of alloy compositions, selection for specific environments, and atmospheric corrosion of selected copper alloys. The article also tabulates the corrosion ratings of wrought copper alloys in various corrosive media.

You do not currently have access to this chapter.
Don't already have an account? Register

1998. "Corrosion Characteristics of Copper and Copper Alloys", Metals Handbook Desk Edition, 2nd Ed., Joseph R. Davis

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal